回复 15# dwfhn 的帖子欢迎交流
欢迎交流:我公司的一个客户没有硬度要求,但有如下要求:
ASTM(美国材料试验协会)E384,材料显微硬度的标准测试方法
ASTM E384, Standard Test Method for Microhardness of Materials
ASTM(美国材料试验协会)E18,材料金属的洛氏硬度和洛氏表面硬度的标准测试方法
ASTM E18, Standard Test Methods for Rockwell Hardness and Rockwell Superficial
Hardness of Metallic Materials
AMS 2753, 渗氮, 液体盐浴, 无氰化物盐浴
AMS 2753, Nitriding, Liquid Salt Bath, Non-Cyanide Bath
硬化层深度 - 是指表面以下至最低硬度为HRC 50或HK542(努氏硬度)处的最大深度。硬化层包括Epsilon相表层和化合(扩散)层。
Case Depth - is the maximum depth below the surface at which a minimum hardness
equivalent to 50 HRC or 542 HK (Knoop Hardness) is achieved. The hardened case
depth includes the top epsilon layer and the compound (diffusion) layer.
Case Depth - shall be 40 microns minimum for stainless steels (such as 410 or 17-4PH)
and shall be 20 microns minimum for low carbon steels (such as AISI 4130 or AISI
4140). Case depth shall be determined by a Knoop microhardness surveys per ASTM
384, latest revision, on metallographically prepared specimens or parts. |
|